I ran electrolysis again today and even the 40 degree temps, it was effective. I have found, that when I combine it with an evaporust soak, it really cleans the metal. Check out the pic.
This bracket was run in the tank for about 10 hours and then soaked in Evaporust. I did not use any other derusting treatment (like a wire brush). Within minutes of the Evaporust soak, it looked like it does now. ![]() |
![]() |
![]() |
![]() |